CM Furnaces Inc.
Model 1704FL laboratory furnace is the newest addition to the CM line of rapid temperature furnaces and is manufactured with a 110 V power supply and standard outlet plug. Rated to operate continuously at 1700 C (3090 F), this furnace has high-purity alumina fiber and Kanthal Super 1800 molydisilicide heating elements for rapid heat up and cool down rates. The 4 in. x 4 in. x 4 in. (100 x 100 x 100 mm) heated chamber can accommodate most laboratory applications. Programmable ramp/soak control and independent over-temperature protection are standard as well as type B thermocouples.