United Defense To Purchase Ceramic Supplier
February 19, 2004
No Comments
United Defense Industries Inc., Arlington, Va., reached an agreement to acquire Cercom Inc., Vista, Calif., an advanced ceramics materials producer and supplier of lightweight ceramic armor. In addition to body armor for soldiers and ceramic armor tiles for vehicles and aircraft, Cercom provides specialty products for semiconductor manufacturing and metal processing. United Defense expects to retain the current team at Cercom.