Seco/Warwick Corp.
Universal HPQ(tm) high pressure quench furnaces with optional low-pressure vacuum carburizing provide the process functionality of standard furnaces with high-pressure quenching including hardening, tempering, annealing, aging, solution heat treatment, brazing and sintering operations in a single furnace, combined with low-pressure vacuum carburizing. The vacuum carburizing option includes FineCarb(r) control system, which provides accurate process control for both low-pressure vacuum carburizing and vacuum high-pressure quenching. It is suitable for large and short-run production requirements.
High-Pressure Quench Furnaces
June 11, 2003
No Comments