Ametek Specialty Metal Products Upgrades Facility
July 28, 2003
No Comments
Ametek Specialty Metal Products placed an order with Rad-Con, Inc., Cleveland, Ohio, to upgrade its metal strip, thermal management products and wire facility in Wallingford, Conn. to 100% hydrogen anneal. The new equipment, which is expected to be operational in the third quarter of 2003, will allow Ametek to improve its annealing capabilities across a broad range of products.