Bodycote Ipswich Installs Vacuum Furnace
Bodycote Ipswich, Ipswich, Mass., installed a bottom loading vacuum furnace from GM Enterprises, Corona, Calif. The vertical furnace can process load sizes up to 5,000 lb. The equipment is capable of pressure quench up to 2 bar with argon. Bodycote Ipswich specializes in vacuum heat treating of formed sheet metal components and the vacuum brazing of complex assemblies. In addition, Bodycote Thermal Processing Inc. has moved its corporate offices to a new Dallas location. The offices can now be reached at 5001 LBJ Fwy, Suite 800, Dallas, TX 75244; tel: 214-904-2420; or fax: 214-904-2424.