Cam Followers with self-lubricating Graphalloy(r) bushing outperform grease lubricate cam followers in high temperatures (to 1000 F) and hostile environments. Graphalloy, a graphite/metal alloy, contains no oil or grease to harden, has a low constant coefficient of friction and eliminates galling or seizing in hot and dry conditions, providing trouble-free operation in ovens and furnace doors, control arms and oven try supports. Under high temperatures or under load, Graphalloy will not soften or extrude. Insoluble Graphalloy works in acids, hydrocarbons, liquid gases and other hostile non-lubricating environments.