This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Formulation Coating
July 6, 2000
ZYP Coatings, Inc.
The NDB STOP-OFF formulation coating can be used with both carburizing and nitriding processes including fluidized bed, vacuum and gas, salt bath and pack. This water-based stop-off paint simplifies use for heat treaters since one product works for all processes. It can also be used to control scaling and decarburization. The paint is effective for 8160 alloys.
Share This Story
You must login or register in order to post a comment.
Report Abusive Comment