The Department of Energy's Office of Industrial Technologies (OIT) has released a report entitled Energy and Environmental Profile of the U.S. Steel Industry. The report presents data for the steel industry as a whole and at a process level for several energy-intensive products. The report characterizes air emissions, effluents, and other residuals generated by each process; provides estimates of quantities; and describes existing treatment and control technologies.