T-M Vacuum Products Inc.
The Super, Pacer and Performer Series vacuum furnace line now includes medium vacuum furnace systems for heat treating mild steel and high-speed steel. The Tool Room series is available with 2-bar or optional 6-bar gas quenching systems. The Heat Treat series includes system hot zones from 9 to 36 ft3 (0.25 to 1 m3) with a mechanical pump/blower system (diffusion pump optional) and with inert gas quenching. All systems include full automatic and programmable controls using a process logic controller (PLC) and a digital control programmer for user friendly, consistent and repeatable cycling.
Vacuum Furnace Systems
June 11, 2003