Alloy Source Book
April 7, 2003
No Comments
Rolled Alloys, Temperance, Mich., offers a revised and updated AL-6XN alloy source book. First published in 1995, the new book incorporates extensive corrosion data, mechanical and physical properties, welding guidelines and fabrication information. Designs stress information and a comprehensive index of ASME/ASTM specifications also are included. AL-6XN alloy is a super-austenitic stainless steel offered in product forms from plate and sheet to pipe, fittings, flanges and appropriate welding consumables.