Morgan Construction Installs Radiant Box Furnace
August 18, 2003
No Comments
Electra Products and the Magnetic Specialties Division of Solar Manufacturing, both of Telford, Pa., installed an Electra Products Series 2500 radiant box furnace at Morgan Construction in Worcester, Mass. The electric furnace is designed to heat workloads in multiple heating zones with silicon carbide elements. The furnace installation increases Morgan's pipe-bending capacity, allowing them to better meet the demand for replacement coiled rod guides.