Techint Technologies installed a hot-rolled products processing line at Sidor. The 400 m/min recoiling line, equipped with skin pass mill supplied by Mino, can process 600 tons/year of coils, 21 tons each max with thicknesses from 1.6 to 6.5 mm.
Techint Technologies (Genoa, Italy; http://www.techint-technologies.com) installed a hot-rolled products processing line at Sidor. The 400 m/min recoiling line, equipped with skin pass mill supplied by Mino, can process 600 tons/year of coils, 21 tons each max with thicknesses from 1.6 to 6.5 mm. The main purpose of the line is to condition and flatten hot-rolled coils for direct use by customers who require good surface and dimensional quality. The installation was completed in two months.
New Techint Processing Line Opened at Sidor
April 22, 2005