Accumet Materials Co.
The CERAM-T family of ceramics is designed to resist thermal shock at temperatures up to 3272¯F (1800¯C). Unlike alumina ceramics, the CERAM-T stands up to sudden temperature changes and exhibits good mechanical properties. The parts are manufactured by slip casting, which allows production of complete shapes to customer supplied drawings.
Alumina Titania Composites
September 5, 2000