Kolene Corporation, Detroit, MI, is offering literature on improving the wear and corrosion resistance of steel and cast iron components. The KoleneR Nu-TrideR ferritic nitrocarburizing process produces an epsilon nitride zone with a subadjacent nitrogen-rich diffusion zone to enhance the engineering properties of ferrous metals.