Materialography
September 5, 2000
No Comments
Structure 35, the Struers Journal of Materialography, 2000, is available from Struers Inc., Cleveland, OH. Articles provide in-depth coverage on a variety of topics including metallographic preparation of metal foams, the true microstructure of materials, formation of nitride layers in the nitrocarburizing of engine valves; pull-out during grinding of ceramics containing an amorphous phase, and a universal grinding disc for the plane grinding of materialographic specimens.