Athena Controls

The TudorT Model 5018 thermocouple, part of the Duratherm IVR line of high temperature vacuum furnace thermocouples, is designed to provide an alternative to refractory metal sheath-type units. It conforms to the requirements of AMS-2750-C and can be used for sensing temperatures up to 3200¯F (1760¯C), depending on the element specified. Type K, R, S, N, or B elements are available as standard with other element types available on request. The thermocouple has a high-purity (99.7%) alumina tube with a quick-connect plug and mating female jack as standard. A 1/2" NPT process thread connector is available as an option.