Dana Corp. Awarded Patent for Plasma-Assisted Metal Joining Technology
June 13, 2005
No Comments
Dana Corp. (Toledo, Ohio; http://www.dana.com) has been awarded the first patent for its AtmoPlas™ microwave atmospheric plasma heating technology. The patent is for plasma-assisted joining of metal components. Dana is currently testing samples for brazing with its customers and is currently exploring additional applications.