The company's stationary metal analyzers (SPECTROLAB and SPECTROMAXx) are now being shipped with a new excitation system. The new SPECTRO plasma generator is the foundation for the optimization, improving the excitation technique required to analyze metal samples. It is based totally on digitized circuit technology, resulting in better reproducibility and a higher degree of accuracy in measurements. The system forms an average discharge of 200 us based on up to 400 segments, and its 125 mW measuring resolution is approximately eight times higher than that of conventional technologies.