Vacuum Furnace Technology
February 9, 2004
No Comments
Seco/Warwick Corp., Meadville, Pa., released brochure V-405 describing its vacuum carburizing systems with single chamber, double chamber and multichamber design configurations that provide both batch and semicontinuous operation capabilities. Information and curves are provided to describe carburizing results documented by the company and the benefits of vacuum carburizing compared with traditional atmosphere carburizing.