The consortium lead by VAI was awarded a contract for the supply of a continuous annealing line for Rasselstein Hoesch GmbH in Andernach, Germany. The consortium is formed by VAI and Drever. Drever International S.A. will supply the annealing furnace and cooling section. The equipment is designed for a maximum production of 80 t/h of tin plate. The line is scheduled to go in production by the middle of 2005.