This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies
By closing this message or continuing to use our site, you agree to our cookie policy. Learn More
This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Industrial Heating logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Industrial Heating logo
  • Home
  • Magazine
    • Digital Magazine
    • Current Issue
    • Archives
  • News
  • Featured
    • IH Daily
    • IH MagEzine
    • Web Exclusives
    • IH Economic Indicators
    • The History of Industrial Heating
    • Heat Treatment Processes
    • Top 10 Heat-Treated Holiday Gifts
  • Topics
    • Additive Manufacturing / 3D Printing
    • Ceramics & Refractories / Insulation
    • Combustion & Burners
    • Heat Treating
    • Heat & Corrosion Resistant Materials / Composites
    • Induction Heat Treating
    • Industrial Gases & Atmospheres
    • Materials Characterization & Testing
    • Melting / Forming / Joining
    • Process Control & Instrumentation
    • Sintering / Powder Metallurgy
    • Vacuum / Surface Treatments
  • Columns
    • Editorial
    • The Heat Treat Doctor
    • Federal Triangle
    • MTI Profile
    • Academic Pulse
    • Heat Treat 5.0
    • International – Brazil
    • Next-Gen Leaders
    • Reshoring Initiative
    • Washington Watch
  • Directories
    • Equipment Buyers Guide
    • Commercial Heat Treat Capabilities Directory
    • Aftermarket Parts & Services Directory
    • Materials Characterization & Testing Equipment Directory
    • Take a Tour
  • More
    • Classifieds
    • White Papers
    • Industrial Heating Bookstore
    • Organizations
    • Market Research
    • Custom Content & Marketing Services
    • FORGE Magazine
    • Continuing Education
  • Multimedia
    • Podcasts
    • Videos
    • Webinars
    • Image Gallery
    • eBooks
  • Events
    • Meetings & Trade Shows
    • FNA
    • Heat Treat Show
  • Blog
    • Dan Herring - Heat Treatment
    • David Pye - Metallurgy
    • Dan Kay - Brazing
    • Debbie Aliya - Failure Analysis
    • Thomas Joseph - Intellectual Property
    • Omar Nashashibi – Government
    • Reed Miller – Thermal Processing
  • Contact
  • Advertise
  • Subscribe
    • Digital Edition Subscriptions
    • eNewsletter
    • Online Registration
    • Customer Service
Home » Insulation Board Material

You have 0 Articles Left This Month. Register Today for Unlimited Access.

Insulation Board Material

January 11, 2004
Order Reprints
No Comments

Thermal Ceramics Inc.

TR-19HS Block is a high-strength, 1900 F (1040 C) structural insulation board material. The medium density (36 pcf), vermiculite composition product has a typical cold crushing strength of 350 psi and is resistant to direct flame exposure or cryolite vapor attack. It can be easily cast or gunned on with refractory castables as well as used with firebrick, refractory plastic or ceramic fiber linings.

You have 0 complimentary articles left.

Register for free today to continue reading!

Already have an account? Sign in here.

Privacy Policy

Related Articles

Methods of Assessing Monolithic Refractories for Material Selection in Aluminum Melt-Hold Furnaces

Ceramics & Refractories/Insulation: Microporous Insulation - A Little Goes a Long Way

Comparing Vacuum Furnace Graphite-Felt Insulation – PAN vs. Rayon

Ceramic Fiber Board

Subscribe For Free!
  • Digital Edition Subscriptions
  • eNewsletters
  • Online Registration
  • Subscription Customer Service

 
More Videos

Popular Stories

012121-Lordstown

Lordstown Motors’ Unprecedented Preorders

ih0121-mcnt-fig1-900

Ultrasonic Techniques for Detecting High-Temperature Hydrogen Attack

ih0121-hcrmc-fig1-900

Advanced Materials Technology: Making a Difference

ih0121-past-photo2-900

Heat Treating: Past, Present and Future

ih0121-reshoring-900

Moser on Manufacturing

10.29 IH SVT 360X180_NEWcustomcontent

Events

February 16, 2021

Materialographic Preparation of Thermal Spray Coating Samples

With the development of new alloys for coatings, it is even more important than ever to understand how something as generic as sample preparation can affect the evaluation of a coating

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.
View All Submit An Event

Poll

Additive Manufacturing

Has additive manufacturing had any impact on your business?
View Results Poll Archive

Products

Practical Heat Treating: Basic Principles

Practical Heat Treating: Basic Principles

See More Products

The History of Industrial Heating 1000 BC - Present Day


Industrial Heating Employment Marketplace

Industrial Heating

Cover_Jan22nd_144px

January 22, 2021

View More Create Account
  • Resources
    • List Rental
    • eNewsletter
    • Manufacturing Group
    • News
    • Want More?
    • Featured
    • Product / Event
    • Industry Links
    • Connect
    • Privacy Policy
    • Survey And Sample
  • Privacy
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2021. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing