This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
"Glazes and Glass Coatings" by Richard A. Eppler and Douglas R. Eppler has been published by the American Ceramic Society (ACerS) and focuses on the making of ceramic coatings, their chemical makeup, and their properties. The book includes 125 photos and illustrations, 70 in full color.