Carpenter Technology Corp.
Custom 465R is a premium melted, martensitic, age-hardenable alloy that provides high strength and fracture toughness. In peak age condition, the alloy offers 260 ksi ultimate tensile strength (UTS) and fracture toughness of 70 ksiÃin. At H900 condition, the steel retains higher notch tensile strength and can reduce instrument size and utilize tighter radii.