GSP
The engineered steel shapes have been enhanced with expanded offerings and services for industrial heating. For furnace and heating applications, the range of engineered profiles cover almost anywhere a steel shape or contour is required. Uses include profiles in heat resistant steel for walking beam furnaces and heat exchanger shapes for boiler construction. A variety of contoured precision production techniques are encompassed-hot rolled, cold drawn, and extruded-in a wide selection of material such as conventional steels, stainless, and titanium.
Engineered Steel Shapes
July 28, 2000
No Comments