The forging processes are offered for metal rings in sizes ranging from 1 lb. to 60,000 lbs. with outside diameters from 2" to 240". The rings are produced by both the open die and seamless rolled ring forging processes. Single piece or high volume quantities in ferrous and nonferrous materials can be supplied. Ring-related secondary services are also offered, including in-house heat treating, rough machining, destructive and non-destructive testing, and metallographic analysis.