Can-Eng Furnaces Ltd. shipped and is currently commissioning a large continuous V-8 engine block solution heat treating, precision air quench and artificial aging system.
Can-Eng Furnaces Ltd. (Niagara Falls, N.Y.; http://www.can-eng.com) shipped and is currently commissioning a large continuous V-8 engine block solution heat treating, precision air quench and artificial aging system. This order follows many months of process development work, which focused on Can-Eng's precision air quench (PAQ) technology. This development work was performed at Can-Eng's R&D facility in Niagara Falls, and the system is scheduled to be put into production in early 2005.