Struers

The RepliSet replication system is designed for use in nondestructive testing and inspection. It can transfer the microstructure of a surface to a highly accurate and stable replica and produce a three-dimensional copy of the surface. The replica is subsequently analyzed off-site under laboratory conditions. Replicas can be made of all metallic materials and most other solid materials like ceramics, plastics, glass and concrete with no size, shape or thickness limitations.