Thermal Dynamix Delivers Quench System
Thermal Dynamix (East Granby, Conn.; www.thermaldynamix.com) delivered its third AutoLoad Quench system to a leading supplier of mill supplies and lab equipment in the textile industry. This equipment enables the customer to reconfigure its internal oil quench furnaces to front load/unload salt quench operation. This expands heat treat capabilities by allowing existing internal quench box furnaces to be used for both quench mediums without modification to the furnaces. The system is designed to accommodate 21 in. x 33 in. x 6 in. x 80 lb load and is rail guided to serve five furnaces.