The Grieve Corp.
No. 925 is a gas-heated, 2000 F (1095 C)pallet furnace with workspace dimensions of 30 in. wide x 48 in. deep x 36 in. high (762 mm x 1219 mm x 915 mm) and 700,000 Btu/h power installed in two modulating natural gas burners with a floor-mounted combustion air blower. The unit also includes a 325 cfm intake-pressurizing blower with motorized dampers on the intake and exhaust for accelerated cooling. The furnace has 7-in. (~180 mm) thick insulated walls comprising 5 in. of 2300 F ceramic fiber and 2 in. of 1700 F ceramic fiber. The workload rests on a removable pallet with 7-in. thick insulation, consisting of 4.5-in. thick 2300 F firebrick and 2.5-in. thick 2300 F firebrick. (www.grievecorp.com)