Schwarzkopf Technologies Corp.

Schwarzkopf Technologies featured HPM Hybrid(tm) hot zones featuring combination PLANSEE ML moly hot face and graphite felt insulation shield package; PLANSEE ML molybdenum hot face shielding, heating elements and supports, gas nozzles and miscellaneous hardware; PLANSEE TZM molybdenum hearth assemblies (posts, caps and rails). HPM Hybrids offer nearly the same carbon-free work environment as all-metal zones with the same energy savings of insulated types. HPM (high performance materials) are constructed for high sag resistance, ductility and strength for extended service life and reduced maintenance. (www.stcmetals.com)