ZIRCAR Refractory Composites Inc.
Refractory Sheet Type RS-A moldable is a ceramic fiber reinforced wet blanket insulation that contains no asbestos and can be easily formed into a wide variety of simple and complex shapes. Drying results in a strong rigid shape that can be rewetted to restore the original moldability, and baking irreversibly removes the moldability, leaving the product unaffected by moisture. It can be frozen and thawed repeatedly with no loss in moldability or other properties. The insulation can be dried rapidly, either with a torch or by applying directly to a hot furnace, to make a quick repair of cracks in, or to replace missing, refractories.