Graphite Metallizing Corp.

The new self-lubricating GRAPHALLOY conveyor roll end bearing assemblies are specially designed to provide solutions for conveyors operating in high temperatures where dry running is required or where applying lubricant is difficult. The hex adapter new assemblies consist of a GRAPHALLOY bushing, standard wear washer and flanged sleeve with hex adapter to suit a range of application requirements. It provides trouble-free performance in temperature from -400 to 1000°F. There is no product contamination that may occur due to oil or grease as used with conventional bearings. FDA grades are available. The new assemblies are an easy retrofit for standard conveyor rollers.www.graphalloy.comInfo # 270 or www.IHadinfo.cc