American Stress Technologies Inc.
The CrankScan 600 off-line audit inspection system monitors residual stress from manufacturing processes and detects grinding damage and some heat treating qualities. The unit requires manual loading and unloading of the test piece. A sensor automatically scans the ground surface, and the test information is sent to Rollscan central unit to be analyzed, displayed and stored in software for appropriate process adjustments.