TurnKey Solutions Inc.

A 7 gal/hr (26 liter/hr) electric evaporator has been added to company's line of electric and gas evaporators. The new evaporator, together with the existing 5 gal/hr (19 liter/hr) unit, can boil wastewater down to paste or dry powder without damage to the evaporator. The product's design eliminates hot spots and applies heat evenly to the bottom and to all four sides. Additional gas evaporators are available ranging from 15 to 300 gal/hr (57 to 1135 liter/hr).