Graftech Announces Additional Prototype Products for Use in Computer and Communications Industries
Graftech Inc., Nashville, Tenn., a subsidiary of UCAR International, developed heat sink, heat spreader, heat pipe and thermal tape prototype products for use in the management of heat in various computer and communications applications. The prototypes are additions to Graftech's eGrafT electronic thermal management product line and extend capability beyond thermal interface materials to electronic thermal component applications. Key advantages include significant weight reduction and flexible form relative to competing materials.