Thermal Dynamics

The Cutmaster(tm) 38 3/8-in. (9 mm) cutting system provides 30 amps of output current for faster cutting capability and greater bevel and pierce capability. Its power provides longer arc length for increased visibility, while an improved pilot arc cuts through paint and rust. The system also features auto voltage selection of 120 to 220 input volts, which eliminates switching errors and allows the system to go from job to job without regard for available input voltage.