Ipsen International Installs Vacuum Furnace in Mexico
May 11, 2001
No Comments
Carpenter Mexico has purchased and installed an IpsenR VUTK 524 10-Bar vacuum furnace from Ipsen International, Rockford, Ill., with convection assisted heating and uniform directional cooling for lowest distortion. Carpenter is now capable of heat treating H13 dies to NADCA recommendations, which will accommodate the growing economy in Mexico.