Sensor Products

The Pressurex Pressure PointsR tactile force indicating films are metrology tools used to assess compressive magnitude and distribution between contacting and impacting surfaces. The films are available in sizes ranging from 0.3 to 1 in. (8 - 25 mm) diameter. The pouch has a clear window on one side for viewing the pressure film and a pressure sensitive adhesive on the back, enabling the sensor to be affixed to any surface.