Scot Forge added a new digital image analysis and archiving system in its metallurgical test laboratory at its Spring Grove, Ill., location. The system enhances the company's analytical testing services by creating a system for long-term storage and easy retrieval of images, making analysis and annotation of images more efficient and allowing photographs to be seamlesly incorporated into metallurgical reports. The system also is especially important in helping customers document quality and meet quality standards such as ISO 9000.