CansorbT organic, oil-only absorbent is made of high quality large-fiber sphagnum peat moss. During processing, a bitumen wax is released from within the peat moss fiber, coating the fiber surface to give the product its hydrophobic quality. It can absorb up to eight times its own weight in hydrocarbons and can be used in both marine and land applications.