Woven Wire Cloth
June 7, 2002
No Comments
Cooley Wire Products introduces literature featuring alloy woven wire cloth. Included is a chart on the various sizes of available meshes. Standards are 4mesh.080 (0.17 in. open) and 2mesh.120 (0.375 in. open). Rectangular space cloth also is listed. Materials are 300 series stainless steel and Inconel 600.