HED International Tech Center Adds New Tapecasting Pilot Plant
June 6, 2002
No Comments
HED International, Ringoes, N.J., installed a new PRO-CAST(r) Model TCM-121SM tapecasting machine and pilot plant at its New Jersey Technical Service Center to extend tapecast product development and customer service capability. The pilot plant can produce a precision tape cast film as thin as 10 microns continuously on either a stainless steel conveyor or polymer carrier. Contract tapecasting and product development service also is available.