The DP3000 portable dew point analyzer provides F/C measurement in the range of +20 to -148F (-7 to -100C). Power is universal 90 to 230 VAC with a battery life of 12 hours. Sample line and filters are included, as well as a rugged case designed for the typical heat treatment environment. The analyzer can be used in vacuum, sintering and brazing (nitrogen, nitrogen/ hydrogen, argon atmospheres).