Goodrich Receives Patent for Chrome Coating
March 25, 2002
No Comments
Goodrich Technology Corp., Pittsburg, Calif., received a notice of allowance from the U.S. Patent and Trademark Office for a patent application covering its Permastar(tm) chrome coating process. The process uses a combination of powder coating and physical vapor deposition to achieve a chrome-like appearance while significantly reducing costs and the high proportion of rejects associated with traditional chrome plating.