Williamson Corporation

The PRO 100 series of multiwavelength, noncontact temperature sensors use advanced ESP programming functions to provide "aim and read" capabilities in applications that are not accurately measured using single and dual wavelength sensors. With no field calibration requirements, the multiwavelength series outperforms other sensors in applications involving nongreybody materials such as aluminum, stainless steel, and zinc-coated metals. In addition, the PRO 100's signal-dilution factor allows the sensors to tolerate small and wandering targets, misalignment, dirty lenses, and partially filled fields of view.