Thermcraft Inc.
The cast electric heating elements are designed for aluminum crucible furnaces and magnesium pot furnaces. The element is manufactured with high-temperature ceramic refractory and iron-chrome-aluminum coils. Nickel-chrome alloy, multistrand leads resist work hardening and lead failure due to normal mechanical shock and vibration.
Cast Electric Heating Elements
July 31, 2002