This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
MICROSCAN(r) is a single or dual spindle vertical-scanning system for hardening and tempering a wide variety of parts. Three power ratings are available: 2.5 kW/30 kHz, 15 kW/200 kHz and 45 kW/200 kHz. The system has a built-in solid state power supply with heat station, programmable scanner, control and recirculating quench system. A user-friendly keyboard provides quick set-up and changeover. To simplify set up, upper tooling centers can be adjusted without tools. A selection of standard, quick-change inductor mountings to minimize changeover times are also available. (www.inductoheat.com)