Kanthal AB
Five new grades of Kanthal Super heating elements are now available. Designed for use at high temperatures, the key feature of the new elements is that they work directly in the furnace atmosphere without requiring a muffle to protect them. Suitable for use in nitrogen, hydrogen, vacuum and mixtures of endogas and reducing furnace atmospheres, the elements are ready-made for use in production and laboratory furnaces in the glass, steel, electronics, ceramics and heat treating industries.
Heating Elements
January 10, 2003
No Comments