This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Steel Bearings
May 8, 2001
Graphite Metallizing Corp.
Self-lubricating GraphalloyR graphite/metal alloy bearings and bushings can operate at temperatures to 1000F (540C), eliminating the need for lubricants that burn off in most steelmaking operations. Graphalloy can be submerged in molten metals and other harsh environments, such as jetting water and saturated steam.
Share This Story
You must login or register in order to post a comment.
Report Abusive Comment