Heatbath Corp.
Durawax is a synthetic wax emulsion engineered for use on ferrous and nonferrous metal products and surfaces. It provides indoor corrosion protection exceeding 200 hours of humidity testing (ASTM D-2247) and can be used as a dry film lubricant in metalworking applications. The wax produces a dry, glossy finish, which can be applied to any clean surface at ambient temperature using dip and spray equipment. The typical immersion cycle is 1 to 3 minutes. The product can be used on bare steel or over conversion coatings such as black oxide and phosphates.
Synthetic Wax
April 3, 2001
No Comments